Grade : IC1007

A tough submicron substrate, PVD coated grade. Suitable for threading heat resistant alloys,austenitic stainless steel and hard steel at low to medium cutting speeds.

PropertyValue
ISO Range - P/M/K(P10-P30)(M05-M20)(K20-K40)
ISO Range - N/S/H (H05-H15)(S05-S20)

PropertyValue
Grade or Coating TypePVD
Coating Layers TiAlN


Find group of specific workpiece material (opens in a new window)


Cutting Speed for: 16IR 12 UN IC1007 - 3318604
ISOMaterialMaterial DesignationMaterial ConditionHardnessCutting Speed Recommendations (Vc)
P1Non-alloy steel and cast steel, free cutting steel <0.25%C.Annealed125 HB110-180 m/min
P2Non-alloy steel and cast steel, free cutting steel >=0.25%C.Annealed190 HB100-170 m/min
P3Non-alloy steel and cast steel, free cutting steel <0.55% CQuenched and tempered250 HB100-170 m/min
P4Non-alloy steel and cast steel, free cutting steel >=0.55% CAnnealed220 HB95-160 m/min
P5Non-alloy steel and cast steel, free cutting steel >=0.55% CQuenched and tempered.300 HB90-155 m/min
P6Low alloy and cast steel (less than 5% of alloying elements)Annealed200 HB85-145 m/min
P7Low alloy and cast steel (less than 5% of alloying elements)Quenched and tempered275 HB80-135 m/min
P8Low alloy and cast steel (less than 5% of alloying elements)Quenched and tempered300 HB75-130 m/min
P9Low alloy and cast steel (less than 5% of alloying elements)Quenched and tempered350 HB70-120 m/min
P10High alloyed steel, cast steel and tool steelAnnealed200 HB65-110 m/min
P11High alloyed steel, cast steel and tool steelQuenched and tempered325 HB65-110 m/min
P12Stainless steel and cast steelFerritic/martensitic200 HB75-125 m/min
P13Stainless steel and cast steelMartensitic240 HB70-115 m/min
M14Stainless steel and cast steelAustenitic, duplex180 HB85-150 m/min
N21Aluminum-wrought alloysNot hardenable60 HB105-315 m/min
N22Aluminum-wrought alloysHardenable100 HB85-260 m/min
N23Aluminum-cast alloys <=12% SiNot hardenable75 HB105-315 m/min
N24Aluminum-cast alloys <=12% SiHardenable90 HB90-280 m/min
N25Aluminum-cast alloys >12% SiHigh temperature130 HB55-170 m/min
N26Copper alloys >1% PbFree cutting110 HB65-195 m/min
N27Copper alloysBrass90 HB65-195 m/min
N28Copper alloysElectrolytic copper100 HB50-150 m/min
S31High temp. alloys Fe basedAnnealed200 HB25-40 m/min
S32High temp. alloys Fe basedHardened280 HB20-30 m/min
S33High temp. alloys Ni or Co basedAnnealed250 HB20-30 m/min
S34High temp. alloys. Ni or Co basedHardened350 HB15-20 m/min
S35High temp. alloys. Ni or Co basedCast320 HB10-20 m/min
S36Titanium (pure)Pure190 HB20-30 m/min
S37Titanium alloysAlpha+beta alloys, hardened310 HB15-20 m/min

Site Map

Groove-Turn & Parting  ISO-Turning   Threading   Milling   Hole Making   Reaming   Boring   Tooling Systems   Modular Adaptations  Multifunction Tools 

Terms of Use and Legal Disclaimer   Privacy Statement
© 2024 ISCAR LTD. Manufacturer of Metalworking Tools (Iscar.com) All Rights Reserved