Grade : IC807G

A hard submicron substrate, PVD coated grade. Suitable for parting and turning heat resistantalloys, austenitic stainless steel and hard steelat low to medium cutting speeds.

PropertyValue
ISO Range - P/M/K(P10-P30)(M05-M20)(K15-K30)
ISO Range - N/S/H (H05-H15)(S05-S20)

PropertyValue
Grade or Coating TypePVD
Coating Layers TiAlN/AlTiN+TiN


Find group of specific workpiece material (opens in a new window)


Cutting Speed for: PENTA 24N100J006 IC807G - 3304792
ISOMaterialMaterial DesignationMaterial ConditionHardnessCutting Speed Recommendations (Vc)
P1Non-alloy steel and cast steel, free cutting steel <0.25%C.Annealed125 HB145-245 m/min
P2Non-alloy steel and cast steel, free cutting steel >=0.25%C.Annealed190 HB125-215 m/min
P3Non-alloy steel and cast steel, free cutting steel <0.55% CQuenched and tempered250 HB95-195 m/min
P4Non-alloy steel and cast steel, free cutting steel >=0.55% CAnnealed220 HB110-220 m/min
P5Non-alloy steel and cast steel, free cutting steel >=0.55% CQuenched and tempered.300 HB85-175 m/min
P6Low alloy and cast steel (less than 5% of alloying elements)Annealed200 HB105-185 m/min
P7Low alloy and cast steel (less than 5% of alloying elements)Quenched and tempered275 HB85-175 m/min
P8Low alloy and cast steel (less than 5% of alloying elements)Quenched and tempered300 HB80-165 m/min
P9Low alloy and cast steel (less than 5% of alloying elements)Quenched and tempered350 HB75-155 m/min
P10High alloyed steel, cast steel and tool steelAnnealed200 HB105-175 m/min
P11High alloyed steel, cast steel and tool steelQuenched and tempered325 HB70-145 m/min
P12Stainless steel and cast steelFerritic/martensitic200 HB125-230 m/min
P13Stainless steel and cast steelMartensitic240 HB105-215 m/min
M14Stainless steel and cast steelAustenitic, duplex180 HB85-215 m/min
K15Grey cast iron (GG)Pearlitic/ferritic180 HB90-180 m/min
K16Grey cast iron (GG)Pearlitic/martensitic260 HB85-165 m/min
K17Nodular cast iron (GGG)Ferritic160 HB95-220 m/min
K18Nodular cast iron (GGG)Pearlitic250 HB85-160 m/min
K19Malleable cast ironFerritic130 HB110-215 m/min
K20Malleable cast ironPearlitic230 HB95-180 m/min
S31High temp. alloys Fe basedAnnealed200 HB45-75 m/min
S32High temp. alloys Fe basedHardened280 HB35-60 m/min
S33High temp. alloys Ni or Co basedAnnealed250 HB35-50 m/min
S34High temp. alloys. Ni or Co basedHardened350 HB30-45 m/min
S35High temp. alloys. Ni or Co basedCast320 HB30-40 m/min
S36Titanium (pure)Pure190 HB105-175 m/min
S37Titanium alloysAlpha+beta alloys, hardened310 HB50-75 m/min
H38Hardened steelHardened55 HRC25-60 m/min
H39Hardened steelHardened60 HRC25-45 m/min
H40Chilled cast ironCast400 HB45-65 m/min
H41Cast ironHardened55 HRC40-50 m/min

Site Map

Groove-Turn & Parting  ISO-Turning   Threading   Milling   Hole Making   Reaming   Boring   Tooling Systems   Modular Adaptations  Multifunction Tools 

Terms of Use and Legal Disclaimer   Privacy Statement
© 2024 ISCAR LTD. Manufacturer of Metalworking Tools (Iscar.com) All Rights Reserved